Study on treatment of difficult settling wastewater from tungsten mineral processing
-
摘要: 钨矿选矿过程中加入了大量的水玻璃和油酸,造成废水中残留大量水玻璃,使废水呈现黏稠的胶状,悬浮物难以沉降。目前国内外关于选矿废水处理的研究大多集中在选矿废水中有机选矿药剂的降解和重金属离子的去除,而对难沉降胶体的去除主要以传统的混凝剂聚合氯化铝(PAC)为主。本研究对不同的絮凝剂和助凝剂进行筛选组合并优化实验参数,使处理后选矿废水达到选矿用水水质要求。实验结果表明:基于实际选矿废水水质调研配制的模拟选矿废水pH值为1226,浊度为1 390 NTU,悬浮物(SS)为2 780 mg/L,Zeta电位为-59.9 mV;优化絮凝剂氯化钙(CaCl2)的投加量为500 mg/L,助凝剂1 500万分子量阳离子型聚丙烯酰胺(PAM)的投加量为30 mg/L,450 r/min快速搅拌反应5 min,160 r/min慢速搅拌2 min后静置沉淀20 min,则上清液浊度为7.11 NTU,浊度去除率高达99.48%。Abstract: Large amount of water glass and oleic acid added to the tungsten ore mineral processing resulted in high concentration of water glass residual in the flotation wastewaterThus,the flotation wastewater was gelatinous and it was difficult for the suspended substance to settleResearches at home and abroad about flotation wastewater treatment are focused on the removal of organic mineral process reagent and heavy metalIn the practical mineral flotation wastewater treatment project,polyaluminium chloride(PAC) was generally used as coagulant to remove the suspended substance which was difficult to settleThis paper screened and combined the different coagulant and coagulant aid,meanwhile optimized the experimental parameters to improve the effluent quality and meet the reusable water quality standard requirementsThe experimental results showed the prepared simulated flotation wastewater based on the investigation of actual flotation wasterwater quality had the characteristics as follows:pH was 1226,turbidity was 1 390 NTU,suspended substance was 2 780 mg/L,Zeta potential was -59.9 mV. Calcium chloride(CaCl2) and 15 million molecular weight cationic polyacrylamide(PAM) were selected as the optimum coagulant and coagulant aid,the dosage was 500 mg/L and 30 mg/ L respectivelyUnder the experimental conditions of 450 r/min rapid stirring for 5 min,160 r/min slow stirring for 2 min,followed by settlement for 20 min,the turbidity of the supernatant was 7.11 NTU and the removal rate could reach 99.48%
-
Key words:
- flotation wastewater /
- water glass /
- difficult settling /
- calcium chloride /
- cationic polyacrylamide
-
[1] 边岳CP型碳质吸附剂处理柿竹园多金属矿山选矿废水实验研究[D]. 徐州:中国矿业大学,2018 [2] 何绪文,李静,张硕,等水解-好氧工艺降解选矿废水部分浮选药剂的研究[J]. 水处理技术,2012,38(S1):80-84 [3] He Xuwen,Li Jing,Zhang Shuo,et al. Degradation of some flotation reagents in flotation wastewater by processes of hydrolysis/aerobic [J]. Technology of Water Treatment,2012,38(S1):80-84 [4] 黄进,崔振宇,解田,等磷矿选矿废水中浮选药剂回收与水深度处理的研究[J]. 矿冶,2012,21(2):88-90 [5] Huang Jin,Cui Zhenyu,Xie Tian,et al. Study on recovery of flotation reagent in phosphorite beneficiation wastewater and wastewater further treatment [J]. Mining & Metallurgy,2012,21(2):88-90 [6] 李代会有色金属选矿废水处理技术的应用研究[J]. 世界有色金属,2018(23):184-185 [7] Li DaihuiApplication research of nonferrous metal separation wastewater treatment technology [J]. World Nonferrous Metals,2018(23):184-185 [8] 李淑菲,李强白钨矿浮选研究现状[J]. 矿产综合利用,2019(3):17-21 [9] Li Shufei,Li QiangCurrent research situation of scheelite flotation [J]. Multipurpose Utilization of Mineral Resources,2019(3):17-21 [10] 章丽萍,项俊,严振宇,等O3降解水杨羟肟酸选矿废水机理研究[J]. 矿业科学学报,2019,4(1):79-85 [11] Zhang Liping,Xiang Jun,Yan Zhenyu,et al. Mechanism study on ozonization degradation of salicylhydroxamic acid in flotation wastewater[J]. Journal of Mining Science and Technology,2019,4(1):79-85 [12] 李纯浪,白家源,杨绍辉,等ICP-OES同时测定选矿废水中锌、铜、铅、镉、锰、铬、铁、镍、砷九种重金属元素[J]. 世界有色金属,2019,9(18):210-212 [13] Li Chunlang,Bai Jiayuan,Yang Shaohui,et al. Simultaneous determination of zinc,copper,lead,cadmium,manganese,chromium,iron,nickel and arsnic in mineral processing wastewater by ICP-OES[J]. World Nonferrous Metals,2019,9(18):210-212 [14] 解维伟,曹国强,贺兰鸿,等浮选脱硫的机理及回归分析预测[J]. 矿业科学学报,2018,3(2):201-208 [15] Xie Weiwei,Cao Guoqiang,He Lanhong,et al. Mechanism and regression analysis of flotation desulfurization[J]. Journal of Mining Science and Technology,2018,3(2) :201-208 [16] 刘艳丽,杨晓明,刘峰彪,等某钨钼矿选矿废水水质调研及混凝沉降实验研究[J]. 矿冶,2019,28(5):106-112 [17] Liu Yanli,Yang Xiaoming,Liu Fengbiao,et al. Water quality and coagulation settlement test of mineral processing wastewater from a tungstenmolybdenum mine[J]. Mining & Metallurgy,2019,28(5):106-112 [18] 孙伟,刘令,曹学锋,等白钨矿选矿废水净化回用基础研究[J]. 矿业研究与开发,2013,33(6):91-95 [19] Sun Wei,Liu Ling,Cao Xuefeng,et al. Fundamental research on purification and recycling of flotation wastewater in scheelite [J]. Mining Research and Development,2013,33(6):91-95 [20] 曹兴,黄士兵,李书生,等某白钨矿选矿废水悬浮物沉降效果优化试验[J]. 现代矿业,2016(2): 77-78,85 [21] Cao Xing,Huang Shibing,Li ShushengOptimization experiment of SS sedimentation effect for flotation wastewater from a scheelite ore[J]. Modern Mining,2016(2):77-78,85 [22] 邓双丽,王延锋,亢建华白钨加温精选废水处理技术研究及应用[J]. 中国钨业,2017,32(1):75-78 [23] Deng Shuangli,Wang Yanfeng,Kang Jianhua. Treatment technology for wastewater from scheelites heated processing [J]. China Tungsten Industry,2017,32(1):75-78 [24] 孟庆有,冯其明,欧乐明油酸钠作用下温度对微细粒黑钨矿可浮性和吸附行为的影响[J]. 中南大学学报,2018,25(7):1582-1589 [25] Meng Qingyou,Feng Qiming,Ou LemingEffect of temperature on floatability and adsorption behavior of fine wolframite with sodium oleate [J]. Journal of Central South University of Technology,2018,25(7):1582-1589 [26] 王纪镇,程雅芝,肖雨辰,等油酸钠/TX-100组合药剂对白钨矿的捕收性能及机理研究[J]. 有色金属:选矿部分,2019,5(1):100-104 [27] Wang Jizhen,Cheng Yazhi,Xiao Yuchen,et al. Collecting performance of mixed NaOL/TX-100 for scheelite flotation and its mechanisum [J]. Nonferrous Metals:Mineral Processing Section,2019,5(1):100-104 [28] 王强强白钨、萤石和方解石浮选分离淀粉类抑制剂及抑制机理研究[D]. 赣州:江西理工大学,2018 [29] 张文钲钼矿选矿技术进展[J]. 中国钼业,2008,32(1):1-7 [30] Zhang WenzhengProgress of molybdenum dressing technique [J]. China Molybdenum Industry,2008,32(1):1-7 [31] 李亚峰,金亚斌,刘元Ca2+等3种成分在煤泥凝聚中作用机理的研究[J]. 沈阳建筑大学学报:自然科学版,2007,23(3):473-477 [32] Li Yafeng,Jin Yabin,Liu YuanStudy on the action mechanism of Ca2+ and two other components in coal slime coagulation [J]. Journal of Shenyang Jianzhu University:Natural Science,2007,23(3):473-477
点击查看大图
计量
- 文章访问数: 210
- HTML全文浏览量: 37
- PDF下载量: 81
- 被引次数: 0